The above mentioned articles need approximately 48 hours to gain the final bond
strength after lamination. Therefore washing tests should not be carried
out earlier than 48 hours after lamination. The web adhesive could have splices,
shadowing, i.e. stripes which are due to production process. Splices are marked.
Important: The information provided is to be considered as a recommendation only. The
values can change under different usage conditions. In any case it is
the buyer's responsibility to test and verify the suitability of the
web adhesive for the particular purpose. Liability is limited to the
replacement of web adhesive supplied, not for laminated products.